The injection molding manufacturing process is a very common bulk manufacturing method due to its repeatability, reliability, and relatively low cycle time. However, like any design or manufacturing process, it’s not without potential pitfalls. Every new mold design presents new challenges for mold and part designers alike. Issues with the final product can be caused by part design, material selection, or mold design. Let’s take a look at 5 of the most common injection molding defects and how we can prevent them.
Weld lines occur in plastic parts when two or more melt fronts come together and meet in the middle. This can happen when dealing with a part with multiple injection locations, or holes, or other geometry in the final product. These defects are not always purely cosmetic; weld lines are often the weakest point of an injection molded part because the melt fronts partially solidify when they collide, resulting in much weaker molecular bonding.
Some of the common fixes for weld lines include:
Sink marks are areas of the plastic part that are recessed from the rest of the part due to uneven cooling while the part is in the mold. Once the melt front enters the mold cavity, it comes into contact with the mold wall and starts to cool, causing it to contract and pull away from the mold. These blemishes are purely cosmetic but still undesirable.
Some of the common fixes for sink marks include:
Warping of plastic parts is also caused by uneven cooling as the part sits in the mold. As different parts of the plastic cool at different rates, they start to shrink and can introduce uneven stresses, bending moments, and torsion into the part, leading to deformations that were not expected when the part was originally designed. This can also cause some precision parts to be out of tolerance, leading to scrap and rework.
Some of the common fixes for warpage include:
One of the more serious defects in injection molding is the creation of air traps in the finished part. These air bubbles can result in structural and cosmetic defects when the air that’s originally in the mold has no exit and gets absorbed into the finished part. If the air in the mold gets compressed tight enough and hot enough, it can actually explode, damaging both the mold and the finished part.
Some of the common fixes for air traps include:
The most crippling issue when dealing with injection molding is the short shot or an incomplete fill of the plastic part. These parts are not only cosmetically incorrect, they are almost 100% scrapped and have to be redone. These issues can lead to the mold being recut or reworked, expensive project delays, and massive financial and productivity losses.
Some of the common fixes for short shots include:
Fortunately, SOLIDWORKS Plastics allows for the analysis of parts that are going to be injection molded to screen for all of these defects and more. We can check for short shots, injection pressures, weld lines, air traps, sink marks, and warping! Reach out to us if you think Plastics will help your workflow and let’s design better parts together!
Prevent Plastic Injection Issues From Ever Happening